Exam map: Laboratory processes: investing, flasking, packing, curing, deflasking, finishing, polishing and quality control.
| Step | Key points |
|---|---|
| Investing | Wax pattern embedded in dental stone in the lower half of a flask; separating medium; upper half poured |
| Wax elimination | Boil out wax; clean mould; apply separating medium (e.g. alginate-based) |
| Packing (sclera) | Scleral acrylic mixed to correct powder–liquid ratio; packed at dough stage; trial closures to remove excess (flash) |
| Iris placement | Painted iris disc positioned at marked centre and angle |
| Curing | Water bath curing cycle under clamp pressure; avoid rapid heating (gaseous porosity) |
| Cooling and deflasking | Slow bench cooling; careful removal to avoid fractures |
| Clear (corneal) layer | Front surface cut back over the iris, veins added, clear acrylic applied and cured |
| Finishing | Trim flash; shape edges; smooth with burs, then sandpapers of increasing grit |
| Polishing | Pumice slurry on rag wheel, then polishing compound to high gloss; avoid overheating |
| Quality control | Check for bubbles, cracks, sharp edges, colour, dimensions; clean and disinfect |
| Fault | Cause |
|---|---|
| Porosity (internal bubbles) | Overheating, too rapid curing, undermixing |
| Surface porosity | Insufficient pressure, insufficient dough |
| Crazing | Solvent contact, stress, alcohol |
| Colour shift | Wrong curing, self-cure use, contamination |
| Warping | Rapid cooling, uneven heating |
| Rough back surface | Inadequate finishing; causes discharge |
Dough stage.
Overheating or too rapid curing, undermixing, insufficient pressure.
To avoid stress and warping.
Solvents (including alcohol) and stress.
About once a year, more often if needed.
Answer all, then press “Check my score”. Option order is mixed.
1. Wax is removed from the mould by:
Answer: Boiling out. Wax elimination.
2. Excess material squeezed out during trial closure is called:
Answer: Flash. Trim later.
3. Rapid heating during cure causes:
Answer: Gaseous porosity. Monomer boils.
4. The final high gloss uses:
Answer: Polishing compound on a soft wheel. After pumice.
5. Patients should not clean prostheses with:
Answer: Alcohol or solvents. Crazing.
6. A rough back surface leads to:
Answer: Discharge and irritation. Polish well.
7. The clear corneal layer is added:
Answer: Over the iris after cutting back the front. Encapsulation.
8. Typical adult remake interval is about:
Answer: Every few years (often around 5). Depends on fit and wear.
← M6. Iris and Sclera Painting, Colour Matching | M8. Scleral Shells, Conformers and Special Cases →
5,885 original MCQs, 150 OSCE stations and 800 viva questions for optometry licensing exams (NBEO, OCANZ, OEBC, UK and India), every option explained with a "why not" and a pearl.
How to cite this page
Patel D. Ocularistry Module 7: Processing: Flasking, Curing, Finishing and Polishing. RPC Rounds (Sadbhaav Eye Clinic). Updated November 2026. Available at: https://www.sadbhaavclinic.com/ocularist-m7-processing-flasking-curing-polishing.html. Accessed [date].
Want to know more about treatment? Read about the Eye Department at Sadbhaav or book a consultation with Dr. Dhaval Patel.